Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bapolene® PP5010 Polypropylene, Extrusion Grade

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Bapolene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® PP5010 Polypropylene, Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolene PP5010 is an extrusion PP high impact copolymer with excellent color and processability. It offers extra high impact strength and low temperature properties.Applications: Auto, pipe, profile, tubing, blow molded containers.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
ASTM D-2240
Tensile Strength, Yield 27.6 MPa
4000 psi
2 in/min (50 mm/min); ASTM D638
Elongation at Break >= 500 %
>= 500 %
2 in/min (50 mm/min); ASTM D638
Elongation at Yield 15 %
15 %
2 in/min (20 mm/min); ASTM D638
Flexural Modulus 1.31 GPa
190 ksi
Secant @ 1% strain; ASTM D-790
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C
189 °F
ASTM D648
Descriptive Properties Value Comments
Process Extrusion
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: