Material Notes:
Bapolene PP5061 is a PP Random Copolymer for injection molding. This resin exhibits good clarity and impact properties. This product meets FDA standards for food contact applications.Applications: Housewares, cassette cases, food containers.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 78
78
ASTM D-785
Tensile Strength, Ultimate 24.1 MPa
3500 psi
2 in/min (50 mm/min); ASTM D-638
Tensile Strength, Yield 24.8 MPa
3600 psi
2 in/min (50 mm/min); ASTM D-638
Elongation at Break 550 %
550 %
2 in/min (50 mm/min); ASTM D-638
Elongation at Yield 11 %
11 %
2 in/min (20 mm/min); ASTM D-638
Flexural Modulus 1.17 GPa
170 ksi
Secant @ 1% strain; ASTM D-790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
ASTM D648
Descriptive Properties Value Comments
Process Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Copyright © lookpolymers.com All Rights Reserved