Barlog Plastics KEBAFLEX E 60.1 TPE-V, Shore A60

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Barlog Plastics
Trade Name KEBAFLEX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBAFLEX E 60.1 TPE-V, Shore A60.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TPE-VInformation provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength at Break 5.00 MPa
725 psi
ISO 527-1
Elongation at Break 500 %
500 %
ISO 527-1
Descriptive Properties Value Comments
Resin Type TPE-V