Category Polymer , Thermoplastic , Elastomer, TPE , Polyester TPE , Polyester, TP
Manufacturer Barlog Plastics
Trade Name KEBAFLEX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBAFLEX P D72.1 Polyester-Elastomer, Shore D75.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TPC-ETInformation provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.016 cm/cm
0.016 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.017 cm/cm
0.017 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
Tensile Strength at Break 39.0 MPa
5660 psi
ISO 527-1
Elongation at Break >= 400 %
>= 400 %
ISO 527-1
Charpy Impact, Notched 1.60 J/cm²
7.61 ft-lb/in²
ISO 179-1eA
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 148 °C
298 °F
ISO 75-1/-2
Descriptive Properties Value Comments
Resin Type TPC-ET