Material Notes:
TPE-SInformation provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.046 cm/cm
0.046 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.012 cm/cm
0.012 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Hardness, Shore A 35
35
Tensile Strength at Break 3.40 MPa
493 psi
ISO 527-1
Elongation at Break 430 %
430 %
ISO 527-1
Descriptive Properties Value Comments
Resin Type TPE-S