Bhansali Engineering Abstron AN480V2 Flame Retardant ABS Grade

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Bhansali Engineering
Trade Name Abstron
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bhansali Engineering Abstron AN480V2 Flame Retardant ABS Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Bhansali
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D-792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D-955
Melt Flow 38 g/10 min

@Load 10.0 kg,
Temperature 220 °C
38 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111
111
ASTM D-785
Tensile Strength, Yield 49.03 MPa

@Thickness 3.20 mm
7112 psi

@Thickness 0.126 in
Type 1, 5 mm/min; ASTM D-638
Flexural Yield Strength 69.6 MPa

@Thickness 6.40 mm
10100 psi

@Thickness 0.252 in
ASTM D-790
Flexural Modulus 2.11 GPa

@Thickness 6.40 mm
306 ksi

@Thickness 0.252 in
ASTM D-790
Izod Impact, Notched 1.275 J/cm

@Thickness 6.40 mm
2.388 ft-lb/in

@Thickness 0.252 in
ASTM D-256
1.47 J/cm

@Thickness 3.20 mm
2.76 ft-lb/in

@Thickness 0.126 in
ASTM D-256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
Method A - Annealed; ASTM D-648
Vicat Softening Point 99.0 °C
210 °F
Method B; ASTM D-1525
Flammability, UL94 V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
Certified at 2.2 mm; UL-94