Bisalloy Steels BisPlate HHA Thickness 5-25 mm

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel , Carbon Steel , Low Carbon Steel
Manufacturer Bisalloy Steels
Trade Name BisPlate
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bisalloy Steels BisPlate HHA Thickness 5-25 mm.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A quenched and tempered steel armor plate suitable for use in both military and civil applications where light weight and resistance to ballistic projectiles is required.
Mechanical Properties Metric English Comments
Hardness, Brinell 500
500
Tensile Strength at Break 1640 MPa
238000 psi
Tensile Strength, Yield 1400 MPa

@Strain 0.200 %
203000 psi

@Strain 0.200 %
Elongation at Break 14 %
14 %
in 50 mm GL
Charpy Impact 8.00 - 16.0 J

@Temperature -20.0 °C
5.90 - 11.8 ft-lb

@Temperature -4.00 °F
Transverse
10.0 - 20.0 J

@Temperature -20.0 °C
7.38 - 14.8 ft-lb

@Temperature -4.00 °F
Longitudinal
Component Elements Properties Metric English Comments
Boron, B 0.0020 %
0.0020 %
Carbon, C 0.32 %
0.32 %
Chromium, Cr 1.2 %
1.2 %
Iron, Fe 97 %
97 %
As Balance
Manganese, Mn 0.40 %
0.40 %
Molybdenum, Mo 0.30 %
0.30 %
Nickel, Ni 0.35 %
0.35 %
Phosphorous, P 0.025 %
0.025 %
Silicon, Si 0.35 %
0.35 %
Sulfur, S 0.0050 %
0.0050 %
Descriptive Properties Value Comments
CE (IIW) 0.61
PCM 0.4
Surface Finish Shotblasted