Bohler-Uddeholm BÖHLER S601 (M2 Modified) High Speed Steel For Cold Work Applications

Category Metal , Ferrous Metal , Alloy Steel , Tool Steel , Cold Work Steel
Manufacturer Bohler-Uddeholm
Trade Name BÖHLER
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bohler-Uddeholm BÖHLER S601 (M2 Modified) High Speed Steel For Cold Work Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Properties: Tungs ten-molybdenum high speed steel with ex cel lent toughness and cut ting proper ties, for a wide variety of uses.Applications: Taps, twist drills, reamers, broaching tools, metal saws, milling tools of all types, wood working tools, cold work tools.
Physical Properties Metric English Comments
Density 8.10 g/cc
0.293 lb/in³
Mechanical Properties Metric English Comments
Modulus of Elasticity 217 GPa
31500 ksi
Thermal Properties Metric English Comments
CTE, linear 11.5 µm/m-°C

@Temperature 20.0 - 100 °C
6.39 µin/in-°F

@Temperature 68.0 - 212 °F
11.7 µm/m-°C

@Temperature 20.0 - 200 °C
6.50 µin/in-°F

@Temperature 68.0 - 392 °F
12.2 µm/m-°C

@Temperature 20.0 - 300 °C
6.78 µin/in-°F

@Temperature 68.0 - 572 °F
12.4 µm/m-°C

@Temperature 20.0 - 400 °C
6.89 µin/in-°F

@Temperature 68.0 - 752 °F
12.7 µm/m-°C

@Temperature 20.0 - 500 °C
7.06 µin/in-°F

@Temperature 68.0 - 932 °F
12.9 µm/m-°C

@Temperature 20.0 - 700 °C
7.17 µin/in-°F

@Temperature 68.0 - 1290 °F
13.0 µm/m-°C

@Temperature 20.0 - 600 °C
7.22 µin/in-°F

@Temperature 68.0 - 1110 °F
Specific Heat Capacity 0.460 J/g-°C
0.110 BTU/lb-°F
Thermal Conductivity 19.0 W/m-K
132 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C 0.85 %
0.85 %
Chromium, Cr 4.1 %
4.1 %
Manganese, Mn 0.25 %
0.25 %
Molybdenum, Mo 5.0 %
5.0 %
Silicon, Si 0.35 %
0.35 %
Tungsten, W 6.4 %
6.4 %
Vanadium, V 1.9 %
1.9 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000540 ohm-cm
0.0000540 ohm-cm