Material Notes:
BB412E is a natural, medium molecular weight, medium melt flow rate polypropylene block copolymer with an optimal mechanical properties balance resulting in high stiffness and very good impact strength both at room temperature and at low temperatures. The material is colored grey based on RAL 7032. Applications: BB412E is recommended for pipe extrusion and injection molding of fittings in the application field of: waste water discharge, cable conduit pipes, sewerage, corrugated pipes, and corrugated boards.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 1.3 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.3 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
2.5 g/10 min

@Load 5.00 kg,
Temperature 190 °C
2.5 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
50mm/min; ISO 527-2
Elongation at Yield 8.0 %
8.0 %
50mm/min; ISO 527
Tensile Modulus 1.30 GPa
189 ksi
ISO 527-2
Charpy Impact, Notched 0.500 J/cm²

@Temperature -20.0 °C
2.38 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Processing Properties Metric English Comments
Middle Barrel Temperature 190 - 230 °C
374 - 446 °F
Die Temperature 200 - 230 °C
392 - 446 °F
Melt Temperature 200 - 230 °C
392 - 446 °F
Head Temperature 200 - 230 °C
392 - 446 °F