Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis BL2571 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Borealis
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BL2571 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BL2571 is a high-density polyethylene with high stiffness and high environmental stress crack resistance. This product is intended for blow molding. Applications: household and chemical containers such as detergents, cleaners, motor oils, and Industrial chemicals, bottles and containers up to 10 liters.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.957 g/cc
0.0346 lb/in³
ISO 1183
Environmental Stress Crack Resistance 40 hour
40 hour
Antarox 10%, F50; ASTM D1693-A
Melt Flow 0.20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
1.0 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.0 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
23 g/10 min

@Load 21.6 kg,
Temperature 190 °C
23 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ISO 868
Tensile Strength, Yield 29.0 MPa
4210 psi
50mm/min; ISO 527-2
Elongation at Yield 8.0 %
8.0 %
50mm/min; ISO 527-2
Tensile Modulus 1.25 GPa
181 ksi
1mm/min; ISO 527-2
Flexural Modulus 1.35 GPa
196 ksi
1mm/min; ISO 178
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C
172 °F
ISO 75-2
Processing Properties Metric English Comments
Middle Barrel Temperature 190 - 220 °C
374 - 428 °F
Die Temperature 180 - 220 °C
356 - 428 °F
Melt Temperature 180 - 220 °C
356 - 428 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved