Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis BorECO™ BA222E Polypropylene Block Copolymer for Non-Pressure Pipes

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Borealis
Trade Name BorECO™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BorECO™ BA222E Polypropylene Block Copolymer for Non-Pressure Pipes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BorECO BA222E is a high molecular weight, low melt flow rate polypropylene block copolymer with superior stiffness and excellent impact properties. BorECO BA222E fulfills the requirements according to EN 1852-1/A1 and is a PP-HM (polypropylene high modulus) material.BorECO BA222E is recommended for solid wall non-pressure piping especially in underground drainage and sewerage and soil and waste applications.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.915 g/cc
0.0331 lb/in³
ISO 1183
Melt Flow 0.25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.00 MPa
4786 psi
At 50 mm/min; ISO 527-2
Elongation at Yield 8.0 %
8.0 %
At 50 mm/min; ISO 527-2
Flexural Modulus 1.90 GPa
276 ksi
At 2 mm/min; ISO 178
Charpy Impact, Notched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179/1eA
0.400 J/cm²

@Temperature -20.0 °C
1.90 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Processing Properties Metric English Comments
Front Barrel Temperature 200 - 220 °C
392 - 428 °F
Die Temperature 210 - 220 °C
410 - 428 °F
Melt Temperature 210 - 230 °C
410 - 446 °F
Head Temperature 210 - 220 °C
410 - 428 °F