Borealis BorPEX™ ME2592 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation))

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Molded
Manufacturer Borealis
Trade Name BorPEX™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BorPEX™ ME2592 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation)).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BorPEXME2592 is a natural, high molecular weight, medium density polyethylene for crosslinkable pipes with excellent flexibility. The compound is especially designed for electron beam irradiation crosslinking. The stabilization package is optimized for good processability, easy crosslinking as well as service at high temperatures. Crosslinkable pipes based on BorPEX ME2592 are recommended for floor heating, radiator connections and for domestic hot and cold water supply. Pipes made from BorPEX ME2592 meet drinking water requirements and DIN 16 894 (MD-PEX pipes)Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.936 g/cc
0.0338 lb/in³
Base Resin; ISO 1183
Oxidative Induction Time (OIT) >= 40 min
>= 40 min
210°C; EN 728/AI cup
High Load Melt Index 10 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.00 MPa
3191 psi
At 50 mm/min; ISO 527
Elongation at Yield 10 %
10 %
ISO 527-2
Tensile Modulus 0.840 GPa
122 ksi
ISO 527-2
Flexural Modulus 0.680 GPa
98.6 ksi
At 2 mm/min; ISO 178