Borealis Borecene Compact™ RM8346 Black Linear Polyethylene for Rotational Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Rotational Molded
Manufacturer Borealis
Trade Name Borecene Compact™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borecene Compact™ RM8346 Black Linear Polyethylene for Rotational Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borecene Compact RM8346 is a third generation linear medium density black polyethylene for rotational molding. The narrow molecular weight imparted through metallocene catalyst technology provides an ideal balance of flow and physical properties. Borecene Compact RM8346 is a black version of Borecene RM8343, suitable for diesel fuel tanks. Borecene Compact RM8346 is delivered as new technology powder.Borecene Compact RM8346 contains 1.0% Carbon Black, which is compounded into the polymer. In addition the grade contains an UV stabilizer which gives excellent UV-stability. The polymer contains long-term antioxidant.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.934 g/cc
0.0337 lb/in³
Base Resin; ASTM D1505
ESCR 10% Igepal® >= 200 hour
>= 200 hour
ARM Method
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.3 MPa
2800 psi
At 50 mm/min; ASTM D683 IV
Flexural Modulus 0.558 GPa
81.0 ksi
At 2 mm/min; ASTM D790
Dart Drop Total Energy 200.0 J/cm
0.3746 ft-lb/mil
(-4oF/-20°C); ASTM D3763
Dart Drop 152 g/micron
3860 g/mil
Instrumented Falling Weight (-4°F/-20°C); ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 65.0 °C
149 °F
ASTM D648
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746