Borealis Bormed™ HD810MO Polypropylene Copolymer for Medical Applications

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Borealis
Trade Name Bormed™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Bormed™ HD810MO Polypropylene Copolymer for Medical Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bormed HD810MO is a specially modified polypropylene homopolymer intended for use in medical and medical related applications, which have to be sterilized by radiation. Products molded in HD810MO and radiated by gamma rays at a dose of 25 kGy have a shelf life of a minimum of 5 years, if stored at a temperature below 40°C.Bormed HD810MO is designed for excellent transparency, excellent chemical resistance, good physical properties, and good printability.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.907 g/cc
0.0328 lb/in³
ISO 1183
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 94
94
ISO 2039-2
Tensile Strength, Yield 29.5 MPa
4280 psi
At 50 mm/min; ISO 527-2
Elongation at Yield 13 %
13 %
At 50 mm/min; ISO 527-2
Tensile Modulus 1.10 GPa
160 ksi
At 1 mm/min; ISO 527-2
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ISO 75-2