Borealis Bormod™ HF955MO Polypropylene Homopolymer for Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Borealis
Trade Name Bormod™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Bormod™ HF955MO Polypropylene Homopolymer for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bormod HF955MO is a high modulus polypropylene homopolymer. Bormod HF955MO is especially developed within the proprietary Borstar technology. The grade utilizes the unique Borstar reactor design capabilities for high crystallinity polypropylene production in combination with the specific Borstar nucleation technology. This combination gives Bormod HF955MO an unique balance of properties for high speed injection molding technology allowing fast cycle due to high de-molding temperature as well as reduced cooling time.Bormod HF955MO is designed for fast production of articles for packaging and houseware. Examples include containers and products with medium to long flow lengths, houseware goods for ambient temperature use, rectangular and flat products, caps and closures with integral hinges, and products with thicker wall sections requiring short cycle time.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ISO 2039-2
Tensile Strength, Yield 40.00 MPa
5801 psi
At 50 mm/min; ISO 527-2
Elongation at Yield 6.0 %
6.0 %
At 50 mm/min; ISO 527-2
Tensile Modulus 2.20 GPa
319 ksi
At 1 mm/min; ISO 527-2
Charpy Impact, Notched 0.250 J/cm²
1.19 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 122 °C
252 °F
ISO 75-2
Processing Properties Metric English Comments
Melt Temperature 220 - 260 °C
428 - 500 °F
Mold Temperature 30.0 - 60.0 °C
86.0 - 140 °F