Material Notes:
Borsoft SE410MO is a specially designed modified relatively soft polypropylene heterophasic copolymer with medium melt flow intended for injection moldingBorsoft SE410MO is a tailor made grade designed for easy production of injection molded lids requiring flexibility, high impact strength, and normal copolymer shrinkage without loosing too much stackability properties.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 230 °C
15 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 70
70
ISO 2039-2
Tensile Strength, Yield 20.99 MPa
3045 psi
At 50 mm/min; ISO 527-2
Elongation at Yield 7.0 %
7.0 %
At 50 mm/min; ISO 527-2
Tensile Modulus 1.00 GPa
145 ksi
At 1 mm/min; ISO 527-2
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
ISO 179/1eA
0.600 J/cm²

@Temperature -20.0 °C
2.86 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Impact Test 36.0 J

@Temperature 0.000 °C
26.6 ft-lb

@Temperature 32.0 °F
Total Penetration Energy; ISO 6603-2
39.0 J

@Temperature -20.0 °C
28.8 ft-lb

@Temperature -4.00 °F
Total Penetration Energy; ISO 6603-2
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ISO 75-2
Processing Properties Metric English Comments
Melt Temperature 210 - 260 °C
410 - 500 °F
Mold Temperature 30.0 - 40.0 °C
86.0 - 104 °F