Material Notes:
Borstar BB2581 is a high-density polyethylene intended for blow molding of products with high stiffness and very good environmental stress crack resistance (ESCR).Borstar BB2581 is recommended for household and industrial chemicals such as detergents, cleaners, and motor oils while being recommended for bottles and containers up to 10 liters.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.958 g/cc
0.0346 lb/in³
ISO 1183
ESCR 10% Igepal® >= 100 hour
>= 100 hour
ASTM D1693
Melt Flow 0.40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
1.8 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.8 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
High Load Melt Index 28 g/10 min

@Load 21.6 kg,
Temperature 190 °C
28 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ISO 868
Tensile Strength, Yield 30.00 MPa
4351 psi
At 50 mm/min; ISO 527-2
Elongation at Yield 8.0 %
8.0 %
At 50 mm/min; ISO 527-2
Tensile Modulus 1.30 GPa
189 ksi
At 1 mm/min; ISO 527-2
Flexural Modulus 1.35 GPa
196 ksi
At 1 mm/min; ISO 178
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ISO 75-2
Processing Properties Metric English Comments
Front Barrel Temperature 170 - 190 °C
338 - 374 °F
Die Temperature 175 - 190 °C
347 - 374 °F