Material Notes:
FA7224 has been developed for applications such as: Thin bags with excellent optical and slip properties, and laundry and other textile bags. Contains antioxidant.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
ISO 1183
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Antiblock Level 1100 ppm
1100 ppm
talc; Borealis Method
Slip Level 700 ppm
700 ppm
erucamide; Borealis Method
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 400 %
400 %
ISO 527-3
Film Elongation at Break, TD 650 %
650 %
ISO 527-3
Tensile Modulus 0.180 GPa
26.1 ksi
TD; ASTM D882-A
0.200 GPa
29.0 ksi
MD; ASTM D882-A
Coefficient of Friction 0.15
0.15
Dynamic; ISO 8295
Elmendorf Tear Strength, MD 7.65 g/micron
194 g/mil
ISO 6383/2
Elmendorf Tear Strength, TD 5.097 g/micron
129.5 g/mil
ISO 6383/2
Dart Drop Test 80.0 g

@Thickness 0.0400 mm
0.176 lb

@Thickness 0.00157 in
ISO 7765-1
Film Tensile Strength at Break, MD 20.0 MPa
2900 psi
ISO 527-3
Film Tensile Strength at Break, TD 18.0 MPa
2610 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 111 °C
232 °F
ISO 11357-3
Vicat Softening Point 94.0 °C
201 °F
ISO 306
Optical Properties Metric English Comments
Haze 6.0 %
6.0 %
ASTM D1003
Gloss 110 %
110 %
ASTM D2457