Material Notes:
HB300TF is a polypropylene homopolymer intended for thermoformed packaging applications. This grade is produced using the Borealis nucleating technology. Its increased crystallization temperature allows reduced cycle time and increased output. Applications: HB300TF is recommended for high transparent trays, cups and containers, house ware and thin wall packaging, margarine tubs and dairy containers, mixing with copolymer, and in line and off line thermoforming.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
base resin; ISO 1183
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.5 MPa
5000 psi
ISO 527-2
Elongation at Yield 9.0 %
9.0 %
50mm/min; ISO 527-2
Tensile Modulus 1.70 GPa
247 ksi
1mm/min; ISO 527-2
Flexural Modulus 1.65 GPa
239 ksi
5mm/min; ISO 178
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 164 - 168 °C
327 - 334 °F
DSC; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ISO 75-2
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified