Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis HJ320MO Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Borealis
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis HJ320MO Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HJ320MO is a polypropylene homopolymer intended for injection molding. Its very high melt flow makes it especially suitable for thin-wall packaging and products with long flow length. This grade is characterized by the unique combination of very high flow, excellent stiffness and excellent organoleptic properties. This grade is designed for high-speed injection molding and contains nucleating and antistatic additives. Components molded from this grade show good ejectability and combine excellent stiffness with good transparency and gloss, very good color, excellent organoleptic properties and good impact strength at ambient temperatures. Applications: thin wall containers, closures, and products with thicker wall sections requiring short cycle time.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 55 g/10 min

@Load 2.16 kg,
Temperature 230 °C
55 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ISO 2039-2
Tensile Strength, Yield 38.0 MPa
5510 psi
50mm/min; ISO 527-2
Elongation at Yield 7.5 %
7.5 %
50mm/min; ISO 527-2
Tensile Modulus 1.80 GPa
261 ksi
1mm/min; ISO 527-2
Charpy Impact, Notched 0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
ISO 75-2
Processing Properties Metric English Comments
Melt Temperature 210 - 250 °C
410 - 482 °F
Mold Temperature 30.0 - 40.0 °C
86.0 - 104 °F
Hold Pressure 20.0 - 50.0 MPa
2900 - 7250 psi
Descriptive Properties Value Comments
Injection Velocity high
Users viewing this material also viewed the following: