Borealis MG9641S Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Borealis
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis MG9641S Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MG9641S is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of articles which require good rigidity, good flow properties and high impact strength. Applications: crates, and snow pulcas.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.964 g/cc
0.0348 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ISO 868
Tensile Strength, Yield 27.0 MPa
3920 psi
50mm/min; ISO 527-2
Elongation at Yield 8.0 %
8.0 %
50mm/min; ISO 527-2
Tensile Modulus 1.20 GPa
174 ksi
1mm/min; ISO 527-2
Charpy Impact, Notched 0.600 J/cm²

@Temperature -20.0 °C
2.86 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C
171 °F
ISO 75-2
Processing Properties Metric English Comments
Melt Temperature 210 - 275 °C
410 - 527 °F
Mold Temperature 10.0 - 40.0 °C
50.0 - 104 °F
Descriptive Properties Value Comments
Hold Pressure as low as possible
Injection Velocity as high as possible