Borealis Visico™ ME4425/LE4462 Scorch Retardant Silane Crosslinkable MDPE Track Resistant Cable Insulation

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Extruded
Manufacturer Borealis
Trade Name Visico™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Visico™ ME4425/LE4462 Scorch Retardant Silane Crosslinkable MDPE Track Resistant Cable Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Visico ME4425/LE4462 is a combination of LE4425, a Medium Density Visico base resin and a masterbatch, LE4462, which contains catalyst, carbon black, UV stabilizers and antioxidants. The LE4462 masterbatch accelerates the moisture-induced crosslinking reaction and imparts track resistance, resistance to degradation by ultraviolet light stability to the final product.Visico ME4425/LE4462 is designed for use as a track resistant insulation for the outer layer of Spacer Aerial Cables and as insulation for Partial Insulated Cables. Although it has been used alone as insulation for cables rated at voltages as high as 35kV, it is recommended that a conductor shield such as LE540 be used for cables rated at voltages above 12 kV or where required by the applicable electrical code.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Specific Gravity 0.935 g/cc
0.935 g/cc
ASTM D1928 C/D 1505
Mechanical Properties Metric English Comments
Hardness, Shore D 51
51
ASTM D2240
Tensile Strength, Yield >= 13.8 MPa
>= 2000 psi
Heat Aging (7 days at 121°C); ASTM D638
16.2 MPa
2350 psi
At 20 in/min; ASTM D638
Elongation at Break 255 %
255 %
Heat Aging (7 days at 121°C); ASTM D412
300 %
300 %
At 20 in/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength >= 31.5 kV/mm
>= 800 kV/in
At 40 mils; ASTM D149
Track Resistance 1.08e+6 sec
1.08e+6 sec
Dust and Fog; ASTM D2132
Processing Properties Metric English Comments
Middle Barrel Temperature >= 180 °C
>= 356 °F
Front Barrel Temperature >= 160 °C
>= 320 °F
Die Temperature >= 191 °C
>= 375 °F
Head Temperature >= 190 °C
>= 374 °F