Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer BorsodChem Rt.
Trade Name ONGRO
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BorsodChem ONGRO CPE 4002 N Chlorinated Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
IMPACT MODIFIER FOR PVChigh impact resistancegood processabilityexcellent weather resistanceELASTOMERSvariety of cross-linking technologiesexcellent ozone- and weather resistanceexcellent chemical resistancegood electrical propertiesfreely colorablePLASTIC MATERIALS, FLAME RETARDANT ADDITIVEcompatibility with a large number of polymerssimple mixingoutstanding heat stabilityexcellent weather resistancelow flammabilityplasticizer free flexible systemsInformation provided by BorsodChem Rt.
Physical Properties Metric English Comments
Apparent Bulk Density 0.450 g/cc
0.0163 lb/in³
MSZ ISO 60
Particle Size 600 µm
600 µm
<1% above
Viscosity 2.60e+6 cP

@Shear Rate 200 1/s,
Temperature 190 °C
2.60e+6 cP

@Shear Rate 200 1/s,
Temperature 374 °F
Capillary viscosimeter
Mooney Viscosity 85

@Temperature 120 °C
85

@Temperature 248 °F
ML(1+4); MSZ 11093 ISO 289
Crystallinity <= 1.0 %
<= 1.0 %
Residual; DSC BC HSz 325
Collected Volatile Condensable Material <= 0.30 %
<= 0.30 %
ISO 1269
Mechanical Properties Metric English Comments
Hardness, Shore A 47
47
MSZ ISO 868
Tensile Strength at Break 10.0 MPa
1450 psi
MSZ ISO 527
Elongation at Break 580 %
580 %
MSZ ISO 527
100% Modulus 0.000600 GPa
0.0870 ksi
MSZ ISO 527
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 3.50 °C
38.3 °F
DMA method 1 Hz
Descriptive Properties Value Comments
Chlorine Content, % 40
Heat Stability at 180°C, minutes 8