Braskem BF0323/12HC Blown Film Extrusion Low Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem BF0323/12HC Blown Film Extrusion Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Shrink films; Automatic packaging of liquid products (FFS).Additives: Antiblock, DInformation provided by Braskem.
Physical Properties Metric English Comments
Specific Gravity 0.923 g/cc
0.923 g/cc
ASTM D1505/D792
Thickness 25.0 microns
0.984 mil
Melt Flow 0.32 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.32 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 390 %
390 %
ASTM D882
Film Elongation at Break, TD 1040 %
1040 %
ASTM D882
Elmendorf Tear Strength TD 100 g
100 g
gF; ASTM D1922
Dart Drop Test 100 g
0.221 lb
gF/50%f; ASTM D1709
Film Tensile Strength at Break, MD 40.0 MPa
5800 psi
ASTM D882
Film Tensile Strength at Break, TD 30.0 MPa
4350 psi
ASTM D882
Optical Properties Metric English Comments
Haze 11 %

@Thickness 0.0250 mm
11 %

@Thickness 0.000984 in
ASTM D1003
Gloss 83 %

@Thickness 0.0250 mm
83 %

@Thickness 0.000984 in
60°; ASTM D2457