Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem CP 202XP HECO Polypropylene Heterophasic Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem CP 202XP HECO Polypropylene Heterophasic Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CP 202XP is a high melt flow rate heterophasic copolymer designed to achieve parts with high stiffness and impact strength resistance, low warpage, and excellent surface appearance. Its applications include: household appliances, high stiffness parts, and compounds. It is designed for injection molding processing.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM-D792
Melt Flow 26 g/10 min

@Load 2.16 kg,
Temperature 230 °C
26 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM-D785
Tensile Strength, Yield 32.0 MPa
4640 psi
ASTM-D638
Elongation at Yield 6.0 %
6.0 %
ASTM-D638
Flexural Modulus, 1% Secant 1600 MPa
232000 psi
ASTM-D790
Izod Impact, Notched 0.220 J/cm

@Temperature -20.0 °C
0.412 ft-lb/in

@Temperature -4.00 °F
ASTM-D256
0.700 J/cm

@Temperature 23.0 °C
1.31 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 126 °C
259 °F
ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ASTM-D648
Vicat Softening Point 155 °C

@Load 1.02 kg
311 °F

@Load 2.25 lb
ASTM-D1525