Material Notes:
Description: CP 401HC is a medium melt flow rate heterophasic copolymer, specially designed to achieve high stiffness/impact strength balance. This product offers good surface appearance and processability.Applications: Outdoor and garden furniture. Information provided by Braskem
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792A
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 96
96
ASTM D785
Tensile Strength, Yield 34.0 MPa
4930 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus 1.70 GPa
247 ksi
1% secant; ASTM D790
Izod Impact, Notched 0.250 J/cm

@Temperature -20.0 °C
0.468 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
0.700 J/cm

@Temperature 23.0 °C
1.31 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 124 °C
255 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C
147 °F
ASTM D648
Vicat Softening Point 156 °C
313 °F
10 N; ASTM D1525