Material Notes:
Bottle caps for carbonated beverages.Information provided by Braskem.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 87
87
ASTM D785
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus, 1% Secant 1500 MPa
218000 psi
ASTM D790A
Izod Impact, Notched 0.380 J/cm

@Temperature -20.0 °C
0.712 ft-lb/in

@Temperature -4.00 °F
ASTM D256
0.990 J/cm

@Temperature 23.0 °C
1.85 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 114 °C
237 °F
ASTM D648