Braskem D130C Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem D130C Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: High BulkApplications: Suggested Uses Include Fine Denier Staple Fiber, High Speed Fiber SpinningThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by FDA – Food and Drugs Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 14 g/10 min

@Load 2.16 kg,
Temperature 230 °C
14 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength 37.2 MPa
5400 psi
2 in/min; ASTM D638
Elongation at Yield 9.0 %
9.0 %
2 in/min; ASTM D638
Tenacity 0.274 N/tex
3.10 g/denier
3.3 draw ration, 1,250 m/min roll speed; 225°C spin temperature, D1000/68, ASTM D2256
Flexural Modulus 1.52 GPa
220 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256A
Descriptive Properties Value Comments
Elongation of Fibers (3.3 draw ration, 1,250 m/min roll speed) 45%
225°C spin temperature, D1000/68, ASTM D2256
Suggested Takeup Roll Speed 8202 ft/min