Braskem F0421 D LDPE Blown Film Extrusion Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem F0421 D LDPE Blown Film Extrusion Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LDPE F0421 D is a low-density polyethylene resin. It has high mechanical and impact strength and good processability, sealability, and shrinkage. It contains antioxidant and slip additives. Its applications include shrink films and automatic packaging of liquid products (FFS).
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ASTM-D792
Melt Flow 0.38 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.38 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 260 %
260 %
ASTM-D882
Film Elongation at Break, TD 960 %
960 %
ASTM-D882
Elmendorf Tear Strength TD 140 g
140 g
ASTM-D1922
Elmendorf Tear Strength, TD 5.60 g/micron
142 g/mil
ASTM-D1922
Dart Drop 4.80 g/micron
122 g/mil
ASTM-D1709
Dart Drop Test 120 g
0.265 lb
ASTM-D1709
Film Tensile Strength at Break, MD 30.0 MPa
4350 psi
ASTM-D882
Film Tensile Strength at Break, TD 20.0 MPa
2900 psi
ASTM-D882
Optical Properties Metric English Comments
Haze 15 %
15 %
ASTM-D1003
Gloss 65 %
65 %
Angle 60°; ASTM-D2457
Descriptive Properties Value Comments
Temperature Profile (°C) 170-190
Blown Film Extrusion