Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem GM8260 HDPE Blow Molding Polyethylene Homopolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem GM8260 HDPE Blow Molding Polyethylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HDPE GM8260 is a high-density polyethylene homopolymer that has high molecular weight and was developed for the blow molding segment of large volumes. Its applications include: drums for lubricant oils, multipurpose extrusion, and sheets.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM-D792
ESCR 100% Igepal® 27 hour

@Thickness 2.00 mm,
Temperature 50.0 °C
27 hour

@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Melt Flow 0.42 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.42 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM-D1238
12 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM-D2240
Tensile Strength at Break 38.0 MPa
5510 psi
ASTM-D638
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM-D638
Flexural Modulus, 1% Secant 1160 MPa
168000 psi
ASTM-D790
Izod Impact, Notched 3.30 J/cm
6.18 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ASTM-D648
Vicat Softening Point 127 °C

@Load 1.02 kg
261 °F

@Load 2.25 lb
ASTM-D1525