Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem Green PE SHA7260 Injection Molding High Density Polyethylene

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Braskem
Trade Name Green PE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem Green PE SHA7260 Injection Molding High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SHA7260 is a high-density polyethylene, developed for the injection molding, easy to process and with high productivity. This resin has a good melt flow with high rigidity and hardness. Its narrow molar mass distribution results in a low tendency to warpage. The minimum biobased content of this grade is 94%, determined according to ASTM D6866. Application: Pails & basins, Caps & Closures, Toys, Lids, Thin-walled parts and Housewares.Information provided by Braskem.
Physical Properties Metric English Comments
Specific Gravity 0.956 g/cc
0.956 g/cc
ASTM D792
ESCR 100% Igepal® <= 4.0 hour

@Temperature 50.0 °C
<= 4.0 hour

@Temperature 122 °F
h/F50; Compression molded 2mm notched-plaques; ASTM D1693
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D2240
Tensile Strength, Yield 29.0 MPa
4210 psi
ASTM D638
Elongation at Yield 7.2 %
7.2 %
ASTM D638
Flexural Modulus, 1% Secant 1350 MPa
196000 psi
ASTM D790
Izod Impact, Notched 0.250 J/cm
0.468 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °C
165 °F
ASTM D648
Vicat Softening Point 124 °C
255 °F
10 N; ASTM D1525