Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem Green PE SHE150 Blown Film Extrusion and Cast Film Extrusion High Density Polyethylene

Category Polymer , Film , Renewable/Recycled Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Braskem
Trade Name Green PE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem Green PE SHE150 Blown Film Extrusion and Cast Film Extrusion High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lower greenhouse gas emissions100% made from renewable raw materialsPerformance and Competitiveness: Green Polyethylene has the same characteristics as petrochemical polyethyleneApplications: Raschel; Shading and protecting nets; Ropes.Information provided by Braskem.
Physical Properties Metric English Comments
Specific Gravity 0.948 g/cc
0.948 g/cc
ASTM D792
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ASTM D2240
Tensile Strength at Break 40.0 MPa
5800 psi
ASTM D638
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Flexural Modulus, 1% Secant 1280 MPa
186000 psi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °C
169 °F
ASTM D648
Vicat Softening Point 128 °C
262 °F
ASTM D1525
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved