Material Notes:
Applications: Thin-walled parts and easy mould filling; food and cosmetic packing; toys and household; sealed closures. Information provided by Braskem
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792A
Melt Flow 40 g/10 min

@Load 2.16 kg,
Temperature 230 °C
40 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 96
96
ASTM D785
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
Izod Impact, Notched 0.250 J/cm

@Temperature 23.0 °C
0.468 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C
207 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C
135 °F
ASTM D648
Vicat Softening Point 154 °C
309 °F
-1kg; ASTM D1525