Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem H 401 Cast Film Extrusion Polypropylene

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem H 401 Cast Film Extrusion Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: H 401 is a medium melt flow rate homopolymer polypropylene, additived with slip and antiblocking agents. Designed specially for cast film. This product features good impact strength, excellent transparency and gloss, good slipping and outstanding weldability.Applications: Coil for automatic packaging; Packages for food and textile products. Information provided by Braskem
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792A
Melt Flow 7.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 83
83
ASTM D785
Tensile Strength, Yield 33.0 MPa
4790 psi
ASTM D638
Elongation at Yield 13 %
13 %
ASTM D638
Flexural Modulus 1.40 GPa
203 ksi
1% secant; ASTM D790
Izod Impact, Notched 0.330 J/cm

@Temperature 23.0 °C
0.618 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
198 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °C
126 °F
ASTM D648
Vicat Softening Point 148 °C
298 °F
10 N; ASTM D1525