Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem Idealis 500 High Molecular Weight Polyethylene Powder

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Braskem
Trade Name Idealis
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem Idealis 500 High Molecular Weight Polyethylene Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Braskem Idealis 500 is the only High Molecular Weight Polyethylene resin in powder form specially designed for the compression molding process; Applications range from food handling cutting boards and playground toys to technical parts.Information provided by Braskem.
Physical Properties Metric English Comments
Specific Gravity 0.951 g/cc
0.951 g/cc
ASTM D792
Particle Size 170 µm
170 µm
Average; Dp50; ASTM D1921
Viscosity Measurement 4.7
4.7
Intrinsic in dl/g; ASTM D4020
Molecular Weight 550000 g/mol
550000 g/mol
Braskem
Melt Flow 0.70 g/10 min

@Load 21.6 kg,
Temperature 190 °C
0.70 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 63

@Time 15.0 sec
63

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break >= 30.0 MPa
>= 4350 psi
ASTM D638
Tensile Strength, Yield >= 20.0 MPa
>= 2900 psi
ASTM D638
Charpy Impact, Notched >= 5.00 J/cm²
>= 23.8 ft-lb/in²
Determined with double-notched specimens; ISO 11542-2
Abrasion 80
80
Braskem (PE500 = 100)
Thermal Properties Metric English Comments
Melting Point 136 °C
277 °F
ASTM D3418
Vicat Softening Point 80.0 °C

@Load 5.10 kg
176 °F

@Load 11.2 lb
ASTM D1525
Users viewing this material also viewed the following: