Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem PCD 0440 HECO Polypropylene Heterophasic Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem PCD 0440 HECO Polypropylene Heterophasic Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PCD 0440 is a medium melt flow rate heterophasic copolymer with high impact strength. This resin is designed for steel pipe coating (SPC) and injection molding. Its applications include: automotive parts, battery cases, toys, household appliances, crates, compounds, and steel pipe coating.
Physical Properties Metric English Comments
Density 0.895 g/cc
0.0323 lb/in³
ASTM-D792
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM-D2240
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM-D638
Elongation at Break >= 1000 %
>= 1000 %
ASTM-D638
Elongation at Yield 11 %
11 %
ASTM-D638
Flexural Modulus, 1% Secant 900 MPa
131000 psi
ASTM-D790
Izod Impact, Notched 0.590 J/cm

@Temperature -20.0 °C
1.11 ft-lb/in

@Temperature -4.00 °F
ASTM-D256
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 48.0 °C
118 °F
ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
172 °F
ASTM-D648
Vicat Softening Point 138 °C

@Load 1.02 kg
280 °F

@Load 2.25 lb
ASTM-D1525