Braskem PH 0242 HOMO Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem PH 0242 HOMO Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PH 0242 is a low melt flow rate homopolymer produced by compression molding. This resin exhibits excellent processability and excellent stiffness/impact strength balance. Its applications include compression molding for carbonated beverages bottle caps.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM-D792
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM-D785
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM-D638
Elongation at Yield 10 %
10 %
ASTM-D638
Flexural Modulus, 1% Secant 1600 MPa
232000 psi
ASTM-D790
Izod Impact, Notched 0.290 J/cm
0.543 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 114 °C
237 °F
ASTM-D648
Vicat Softening Point 153 °C

@Load 1.02 kg
307 °F

@Load 2.25 lb
ASTM-D1525