Braskem PH 0952 HOMO Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem PH 0952 HOMO Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PH 0952 is a medium melt flow rate homopolymer with slip and antiblocking agents. This product is designed for technical films and packaging for cast and blown film extrusion. This product features excellent optical properties and good processability. Its applications include: coil for automatic packaging, food and textile packaging, and films for lamination.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM-D792
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM-D785
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM-D638
Elongation at Yield 11 %
11 %
ASTM-D638
Flexural Modulus, 1% Secant 1200 MPa
174000 psi
ASTM-D790
Izod Impact, Notched 0.270 J/cm
0.506 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ASTM-D648
Vicat Softening Point 149 °C

@Load 1.02 kg
300 °F

@Load 2.25 lb
ASTM-D1525