Braskem PRA 0852 RACO Random Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem PRA 0852 RACO Random Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PRA 0852 is a medium melt flow rate random copolymer with slip and antiblocking agents. It is suitable for blown and cast film extrusion. PRA 0852 has excellent optical properties and good processability. Its applications include: flexible packages with excellent gloss, transparency, and sealing properties for general purpose; and food and textile packaging.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM-D792
Melt Flow 8.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM-D785
Tensile Strength, Yield 33.0 MPa
4790 psi
ASTM-D638
Elongation at Yield 9.0 %
9.0 %
ASTM-D638
Flexural Modulus 1.20 GPa
174 ksi
ASTM-D790
Izod Impact, Notched 0.450 J/cm
0.843 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM-D648
Vicat Softening Point 139 °C

@Load 1.02 kg
282 °F

@Load 2.25 lb
ASTM-D1525