Braskem RP 145 RACO Random Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem RP 145 RACO Random Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
RP 145 is a high melt flow rate random copolymer designed for use in thin-walled injection molding parts. This product offers good transparency, very good stiffness/impact strength balance, excellent processability, and has very low odor/taste. Its applications include: packages with excellent organoleptic properties, cosmetic packaging, containers for the freezer, and disposable packages with high transparency.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM-D792
Melt Flow 40 g/10 min

@Load 2.16 kg,
Temperature 230 °C
40 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 83
83
ASTM-D785
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM-D638
Elongation at Yield 16 %
16 %
ASTM-D638
Flexural Modulus, 1% Secant 1000 MPa
145000 psi
ASTM-D790
Izod Impact, Notched 0.180 J/cm

@Temperature -20.0 °C
0.337 ft-lb/in

@Temperature -4.00 °F
ASTM-D256
0.430 J/cm

@Temperature 23.0 °C
0.806 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 79.0 °C
174 °F
ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 49.0 °C
120 °F
ASTM-D648
Vicat Softening Point 127 °C

@Load 1.02 kg
261 °F

@Load 2.25 lb
ASTM-D1525
Optical Properties Metric English Comments
Haze 14 %

@Thickness 1.00 mm
14 %

@Thickness 0.0394 in
ASTM-D1003