Material Notes:
Braskem Symbios 4102 is a medium melt flow rate terpolymer with a heat seal temperature below 120ºC on its treated face. It is designed for use as a heat sealing layer on bioriented films (BOPP) and for film coextrusion. This product does not have slip and anti-blocking agents so it's indicated for customized formularization. This product is appropriate for metallization and lamination processes.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM-D792
Melt Flow 5.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 79
79
ASTM-D785
Film Tensile Strength at Yield, TD 13.0 MPa
1890 psi
ASTM-D882
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM-D638
Elongation at Yield 13 %
13 %
ASTM-D638
Flexural Modulus 0.700 GPa
102 ksi
1% secant; ASTM-D790
Izod Impact, Notched 0.200 J/cm

@Temperature -20.0 °C
0.375 ft-lb/in

@Temperature -4.00 °F
ASTM-D256
0.500 J/cm

@Temperature 23.0 °C
0.937 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 48.0 °C
118 °F
ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °C
165 °F
ASTM-D648
Vicat Softening Point 121 °C

@Load 1.02 kg
250 °F

@Load 2.25 lb
ASTM-D1525