Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem TR3020F Random Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem TR3020F Random Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: High flexural modulus. Applications: Suggested uses include extrusion, blow molding. Process: Extrusion. This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by FDA – Food and Drugs Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 29.0 MPa
4200 psi
2 in/min; ASTM D638
Elongation at Yield 13 %
13 %
2 in/min; ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256A