Material Notes:
Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resistanceHigher melt flow available for improved processibilityProcessing Method: Injection MoldingInformation Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Melt Flow 10 - 20 g/10 min
10 - 20 g/10 min
ASTM D1238
Ash <= 4.0 %
<= 4.0 %
ASTM D5630
Mechanical Properties Metric English Comments
Izod Impact, Notched >= 0.641 J/cm
>= 1.20 ft-lb/in
ASTM D256