Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC 1050 Thermoset Polyester.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC 1050 is a cosmetic, appliance grade material with superior heat stability. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical applications are toaster end panels, iron skirts and lighting baffles.
Physical Properties Metric English Comments
Specific Gravity 1.95 - 2.05 g/cc
1.95 - 2.05 g/cc
Water Absorption 0.12 - 0.18 %
0.12 - 0.18 %
24 hours, 23°C
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm
0.0015 - 0.0025 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 45 - 55
45 - 55
Tensile Strength, Ultimate 34.5 - 48.3 MPa
5000 - 7000 psi
Flexural Strength 82.7 - 110 MPa
12000 - 16000 psi
Flexural Modulus 12.4 - 13.8 GPa
1800 - 2000 ksi
Compressive Strength 124 - 138 MPa
18000 - 20000 psi
Izod Impact, Notched 1.07 - 2.14 J/cm
2.00 - 4.00 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Strength 13.8 kV/mm
350 kV/in
Short Time
Arc Resistance 185 sec
185 sec
Processing Properties Metric English Comments
Mold Temperature 138 - 166 °C
280 - 330 °F