Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bulk Molding Compounds BMC 350 Thermoset Polyester, Medium Impact

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC 350 Thermoset Polyester, Medium Impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC 350 is a cosmetic and appliance grade material with excellent heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical applications are small appliance end panels, control panels, bases and large appliance handles, vent trim and control panels.
Physical Properties Metric English Comments
Specific Gravity 1.85 - 1.95 g/cc
1.85 - 1.95 g/cc
Water Absorption 0.15 - 0.25 %
0.15 - 0.25 %
24 hours, 23°C
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 40 - 50
40 - 50
Tensile Strength, Ultimate 41.4 - 48.3 MPa
6000 - 7000 psi
Flexural Strength 82.7 - 110 MPa
12000 - 16000 psi
Flexural Modulus 11.0 - 12.4 GPa
1600 - 1800 ksi
Compressive Strength 124 - 138 MPa
18000 - 20000 psi
Izod Impact, Notched 1.60 - 2.67 J/cm
3.00 - 5.00 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 218 - 260 °C
425 - 500 °F
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Mold Temperature 138 - 166 °C
280 - 330 °F
Users viewing this material also viewed the following: