Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bulk Molding Compounds BMC 845 Vinyl Ester Molding Compounds, 30% Glass-Filled

Category Polymer , Thermoset , Vinyl Ester
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC 845 Vinyl Ester Molding Compounds, 30% Glass-Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: BMC 845 is designed for use in PEM type fuel cell applications such as end plates and manifolds. It is a corrosion resistant product that shows outstanding creep resistance and compressive creep at elevated temperatures. It can be easily injection compression molded or compression molded depending on the applications requirements. This product is available in bulk and extruded formsInformation provided by Bulk Molding Compounds
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
Linear Mold Shrinkage 0.00 cm/cm
0.00 in/in
Mechanical Properties Metric English Comments
Flexural Yield Strength 138 MPa
20000 psi
Flexural Modulus 13.8 GPa
2000 ksi
Izod Impact, Unnotched 3.74 J/cm
7.00 ft-lb/in
Tensile Creep Modulus, 1000 hours 20.7 MPa
3000 psi
2%
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 HB
HB
Descriptive Properties Value Comments
Color Natural
Users viewing this material also viewed the following: