Bulk Molding Compounds BMC T15(GPS) General Purpose Molding Compound

Category Polymer , Thermoset , Polyester, TS , Polyester (Thermoset) - Rigid
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC T15(GPS) General Purpose Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC T15(GPS) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPS) is well suited for injection, transfer or compression molding of intricate parts. Typical applications are circuit breakers, insulators, bobbins and electrical connectors.Information provided by Bulk Molding Compounds, Inc.
Physical Properties Metric English Comments
Density 1.79 - 1.99 g/cc
0.0647 - 0.0719 lb/in³
Molded
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 30 - 35
30 - 35
Tensile Strength 37.9 - 51.7 MPa
5500 - 7500 psi
Flexural Strength 165 - 193 MPa
24000 - 28000 psi
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Compressive Strength 110 - 138 MPa
16000 - 20000 psi
Izod Impact, Notched 4.16 - 5.23 J/cm
7.80 - 9.80 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 13.8 - 15.7 kV/mm
350 - 400 kV/in
short time
Arc Resistance >= 183 sec
>= 183 sec
Comparative Tracking Index >= 500 V
>= 500 V
Processing Properties Metric English Comments
Processing Temperature 138 - 166 °C
280 - 330 °F