Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bulk Molding Compounds BMC T40(18)V0 Die Casting Replacement Grade Molding Compound

Category Polymer , Thermoset , Polyester, TS , Polyester (Thermoset) - Rigid
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC T40(18)V0 Die Casting Replacement Grade Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC T40(18)V0 is a lower cost version of BMC T40(18) where a UL 5V rating is not necessary.
Physical Properties Metric English Comments
Density 1.72 - 1.92 g/cc
0.0621 - 0.0694 lb/in³
Molded
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm
0.0010 - 0.0020 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 50 - 60
50 - 60
Tensile Strength 62.1 - 75.8 MPa
9000 - 11000 psi
Flexural Strength 131 - 159 MPa
19000 - 23000 psi
Flexural Modulus 7.58 - 8.96 GPa
1100 - 1300 ksi
Compressive Strength 138 - 165 MPa
20000 - 24000 psi
Izod Impact, Notched 4.11 - 5.18 J/cm
7.70 - 9.70 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 13.2 - 15.2 kV/mm
335 - 385 kV/in
short time
Arc Resistance >= 190 sec
>= 190 sec
Comparative Tracking Index >= 500 V
>= 500 V
Processing Properties Metric English Comments
Processing Temperature 138 - 166 °C
280 - 330 °F