Bulk Molding Compounds tetra-DUR F 4001 Bulk Molding Compound

Category Polymer , Thermoset , Polyester, TS , Polyester (Thermoset) - Rigid
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name tetra-DUR
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds tetra-DUR F 4001 Bulk Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UL-Licensed, Abrasion resistance, free of fiber glass.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), thermal stability, color retention, chemical stability, zero shrink/class-A-surface, and uniform color.Information provided by Bulk Molding Compounds, Inc.
Physical Properties Metric English Comments
Density 1.60 - 1.70 g/cc
0.0578 - 0.0614 lb/in³
ISO 1138
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
processing; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength 30.0 MPa
4350 psi
ISO 527
Flexural Strength 55.0 - 80.0 MPa
7980 - 11600 psi
ISO 178
Flexural Modulus 5.00 - 8.00 GPa
725 - 1160 ksi
ISO 178
Compressive Strength 130 - 140 MPa
18900 - 20300 psi
ISO 604
Charpy Impact Unnotched 0.500 - 1.00 J/cm²
2.38 - 4.76 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.300 - 0.800 J/cm²
1.43 - 3.81 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C
16.7 µin/in-°F
VDE 0304T1
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °C
>= 392 °F
ISO 75
Flammability, UL94 V-0

@Thickness 19.0 mm
V-0

@Thickness 0.750 in
Shrinkage <= 0.10 %
<= 0.10 %
post molding; ISO 2577
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Constant 4.5

@Frequency 100 Hz
4.5

@Frequency 100 Hz
IEC 60250
Dielectric Strength 22.0 kV/mm

@Thickness 1.00 mm
559 kV/in

@Thickness 0.0394 in
IEC 60243
Dielectric Loss Index <= 0.040

@Frequency 100 Hz
<= 0.040

@Frequency 100 Hz
IEC 60250
Arc Resistance 180 sec
180 sec
ASTM D495-61
Comparative Tracking Index >= 600 V
>= 600 V
IEC 60112
Descriptive Properties Value Comments
Water Absorption >80 mg/1d
ISO 62