CE Phenolic Laminate

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CE Phenolic Laminate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cotton based phenolic provides more mechanical strength than paper grades and has a finer surface with better machinability. This material is used for gears, pinions, bearings, bushings, and many structural applications.Information provided by Aurora Technologies.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0500 lb/in³
Water Absorption 1.1 %
1.1 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 105
105
Tensile Strength, Ultimate 89.6 MPa
13000 psi
Flexural Strength 131 MPa
19000 psi
Compressive Strength 255 MPa
37000 psi
Shear Strength 68.9 MPa
10000 psi
Izod Impact, Notched 0.961 J/cm
1.80 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 115 °C
239 °F
Electrical
125 °C
257 °F
Mechanical
Electrical Properties Metric English Comments
Dielectric Strength 7.87 kV/mm
200 kV/in
Descriptive Properties Value Comments
Color Natural